Haw. Code R. § 6-77-30

Current through November, 2024
Section 6-77-30 - Yield strength (S) for steel pipe
(a) For pipe that is manufactured in accordance with a specification listed in section I of Appendix B, the yield strength to be used in the design formula in section 6-77-29 is the SMYS stated in the listed specification, if that value is known.
(b) For pipe that is manufactured in accordance with a specification not listed in section I of Appendix B or whose specification or tensile properties are unknown, the yield strength to be used in the design formula in section 6-77-29 is one of the following:
(1) If the pipe is tensile tested in accordance with section II.D. of Appendix B, the lower of the following:
(A) Eighty percent of the average yield strength determined by the tensile tests;
(B) The lowest yield strength determined by the tensile tests, but not more than 52,000 p.s.i.
(2) If the pipe is not tensile tested as provided in subsection (b)(1) 24,000 p.s.i.

Haw. Code R. § 6-77-30

[Eff ] (Auth: HRS § 269-6) (Imp: 49 C.F.R. §192.107, OCT 1, 1990)