49 C.F.R. §§ 179.100-10

Current through October 31, 2024
Section 179.100-10 - Postweld heat treatment
(a) After welding is complete, steel tanks and all attachments welded thereto must be postweld heat treated as a unit in compliance with the requirements of AAR Specifications for Tank Cars, appendix W (IBR, see § 171.7 of this subchapter).
(b) For aluminum tanks, postweld heat treatment is prohibited.
(c) Tank and welded attachments, fabricated from ASTM A 240/A 240M (IBR, see§ 171.7 of this subchapter), Type 304L or Type 316L materials do not require postweld heat treatment, but these materials do require a corrosion resistance test as specified in § 179.100-7(c)(2) .

49 C.F.R. §§179.100-10

Amdt. 179-10, 36 FR 21345, Nov. 6, 1971, as amended by Amdt. 179-47, 58 FR 50238, Sept. 24, 1993; Amdt. 179-52, 61 FR 28679, June 5, 1996; 67 FR 51660 , Aug. 8, 2002; 68 FR 75758 , 75759, Dec. 31, 2003