TABLED. BOTTOM LINER SPECIFICATIONS
Method | Coated Fabric | Extruded Fabric |
Short-term storage of petroleum-contaminated soil (less than 180 days) | ||
Cold crack (ASTM D 2136-02(2012), updated 2012) | -60° Fahrenheit | -60° Fahrenheit |
Black carbon content (ASTM D 1603-14, updated 2014) | two percent or greater | two percent or greater |
Tensile strength (ASTM D 751 -06(2011), updated 2011) | 125 pounds (warp) | N/A |
Mullen burst (ASTM D 751-06(2011), updated 2011) | 250 pounds per square inch (psi) | N/A |
One inch tensile strength (ASTM D 882-12, updated August 2012) | N/A | 25 pounds (warp) |
One inch elongation MD (machine direction) | N/A | 550 percent |
Nominal thickness | 10 mils | 10 mils |
Oil resistance (ASTM D 471- 12a, updated December 2012) | No signs of deterioration and more than 80 percent retention of tensile and seam strength after immersion for 30 days at 73° Fahrenheit | No signs of deterioration and more than 80 percent retention of tensile and seam strength after immersion for 30 days at 73° Fahrenheit |
Long-term storage of petroleum-contaminated soil (180 days to two years) | ||
Cold crack (ASTM D 2 136-02(2012), updated 2012) | -60° Fahrenheit | -60° Fahrenheit |
Black carbon content (ASTM D 1603-12, updated May 2012) | two percent or greater | two percent or greater |
Tensile strength (ASTM D 751-06(2011), updated 2011) | 300 pounds (warp) | N/A |
Mullen burst (ASTM D 75 1-06(2011), updated May 201 J) | 500 pounds per square inch (psi) | N/A |
One inch tensile strength (ASTM D 882-12, updated August 2012) | N/A | 45 pounds (warp) |
One inch elongation MD (machine direction) | N/A | 625 percent |
Nominal thickness | 20 mils | 20 mils |
Oil resistance (ASTM D 471- 12a, updated December 2012) | No signs of deterioration and more than 80 percent retention of tensile and seam strength after immersion for 30 days at 73° Fahrenheit | No signs of deterioration and more than 80 percent retention of tensile and seam strength after immersion for 30 days at 73° Fahrenheit |
The ASTM International methods referred to in this table are adopted by reference. "N/A" means not applicable. |
18 AAC 75.370
The ASTM International methods adopted by reference in Table D of 18 AAC 75.370(a) may be reviewed at the department's Anchorage, Fairbanks, Juneau, and Soldotna offices, or may be obtained from ASTM International, Publications Department, 100 Barr Harbor Drive, P.O. Box C700, West Conshohocken, Pennsylvania 19428-2959; telephone (610) 832-9585; fax (610) 832-9555, or at www.astm.org.
As of Register 215 (October 2015), the regulations attorney made technical corrections under AS 44.62.125(b)(6), to 18 AAC 75.370(a), Table D.